Iron removal from a kaolinitic clay by leaching to obtain high whiteness index



Legorreta García, Felipe

2013

R A Hernandez Hernandez, F Legorreta Garcia, L E Hernandez Cruz, A Martinez Luevanos, ?Iron removal from a kaolinitic clay by leaching to obtain high whiteness index? (2013) IOP Conf. Series: Materials Science and Engineering 45 (2013) 012002 doi:10.1088/1757-899X/45/1/012002


Abstract


Beige kaolin clays were crushed and sieved. The mineral was characterized by X-ray diffraction and chemically analyzed by atomic absorption spectrophotometry. The material below 37 microns was leached with oxalic acid. A study of main variables of the leaching process in different ranges was realized: time (0 to 120 min), temperature (25 to 100 C) and acid concentration (0.01 to 0.5 M). Crystallographic analysis of the initial sample indicates the presence of kaolinite, iron oxides in the form of magnetite and iron-titanium oxides. By this method it was possible to obtain iron extraction percentages over 80% and whiteness index above to 90%.



Producto de Investigación




Artículos relacionados

Síntesis y estudio de resonancia paramagnética electrónica de CaMnO3 y Eu0.05Ca0.95MnO3 obtenidos po...

Purificación del caolín por electrólisis

ESTUDIO DE LA MANGANITA EuxCa1-xMnO3

ESTUDIO DE LA SÍNTESIS Y CARACTERIZACIÓN DE LA MANGANITA DE CALCIO DOPADA CON LANTANO OBTENIDA POR C...

PURIFICACIÓN DE CAOLÍN POR ELECTRÓLISIS

OBTENCIÓN DE POLVOS CERÁMICOS DEL SISTEMA EuxCa1-xMnO3 POR EL MÉTODO POLIOL

ESTUDIO DEL EFECTO DE LA TEMPERATURA DE SÍNTESIS EN LA ELABORACIÓN DE MANGANITAS DE CALCIO DOPADAS C...

ESTUDIO COMPARATIVO DEL USO DE ÁCIDO CÍTRICO Y UREA EN LA SÍNTESIS DE MANGANITAS DE CALCIO DOPADAS C...

BENEFICIO DE CAOLÍN PROCEDENTE DEL MUNICIPIO DE AGUA BLANCA POR FLOTACIÓN INVERSA: PRUEBAS PRELIMINA...

SÍNTESIS DE NANOCOMPÓSITOS DE ZrO2-NANOTUBOS DE CARBONO-Mo.